Heat Treatment steel strip

Categories: ,

Manufacturing range

Material Specification(mm) Mechanical Properties
S35C ~ S80C
Thickness : 0.3 ~ 3.2
Width : 50 ~ 550

Hardness:   

- HV 280 ~ 700

Tensile strength:   

- Martemering : 1,600 ~ 2,100 N/㎟

- Austempering : 1,200 ~ 1,400 N/㎟

- Patenting(SK-5) : 1,100 ~ 1,300 N/㎟

SK steel(2M~5M)
SCM steel
SKS steel
50CrV4

Surface finish

Category Surface Finish
Bright hardened
Condition of Bright Heat Treatment Only
Polished finish
Condition of Polishing after Heat Treatment
Blue or Yellow
Condition of Bright Heat Treatment Only
White polished
Condition of Polishing after Heat Treatment

Manufacturing

Heat treatment method Internal organization Tensile Strength Use Remarks
Martempering
Martensite
1,500 ~ 2,000 N/㎟
- Saw Blade
- Circular Saw
- Spring
- Instrument of Trowel and Others
- Car Components (Sort of Clutch and others)
- Universal products
- Use is the most various
Austempering
Bainite
1,350 N/㎟
- Material for Car Precision Components
-- Clutch, cushion Plate
- Punching dies
(For Paper, Leather)
- For Precision Components of OA Instruments
- Materials available to cooling plastic
Patenting
Sorbite
Condition of material re-rolling 1,200 → 2,400 N/㎟
- High Strength Spring
(Seat Belt Springs)
- The need of re-rolling
(Over 80%)

Product Use (Applications)

Martempering
Hand Saws

Circular Saw Blades

Band Saws

Reaper blades

Austempering
Cusion plate

Patenting
Seat belt spring

High-strength spiral springs